Contractions or density changes of chilled lead glass samples caused by heating them at constant temperatures in the temperature range from 150° to 500°C, were observed by both interferometric dilatometer and sink-float method for measuring density. By comparing the time-contraction relations at various temperatures with the equations proposed by Tool, Ritland or Kanai and Sato, it was found that these equations did not hold exactly in the abovementioned temperature range which is lower than that examined by the above authors. It was supposed that there must be several mechanisms which cause this density change, and the mechanism which contributes mainly to the density change must be different for different range of temperatures.
- 1957-08-01
論文 | ランダム
- 通信処理用高速テーブル検索モジュールの検討
- 高等植物におけるNudix hydrolaseファミリーの多様な生理機能--ヌクレオシド2-リン酸類縁体の代謝を介した細胞応答制御
- 植物の環境ストレスに対する熱ショック転写因子HsfA2を介した応答・適応機構
- 1-II-6 シロイヌナズナADP-ribose/NAD(P)H pyrophosphohydrolase,AtNUDX7,による酸化的DNA損傷修復機構の制御(一般研究発表,日本ビタミン学会第61回大会研究発表要旨)
- 1-II-7 NADPH pyrophosphohydrolase(AtNUDX19)を介した葉緑体でのNADPH代謝が光環境順応に及ぼす影響(一般研究発表,日本ビタミン学会第61回大会研究発表要旨)