ローラチェーンリンクプレートの疲労および衝撃強度に及ぼす熱処理の影響
スポンサーリンク
概要
- 論文の詳細を見る
In this report, the fatigue strengtn and impact strength of roller chain link-plates subjected to various conditions of heat treatment are shown. The experimental results are as follows : (1) The most favorable condition for heat treatment of roller chain link-plates for their fatigue strength will be that the link-plates will be first hardened and tempered, and then austempered and tempered, and that the temperature will be 370℃, H_<RA> 72 for both tempering and austempering. (2) For resistance to repeated impact energy from 20 Kg・cm to 50 Kg・cm, the most favorable condition for heat treatment of link-plates will be that the link-plates will be austempered, and that the temperature for austempering will be 370℃ and H_<RA> 72. (3) The link-plates of H_<RA> 78 have proved strongest for repeated impact energy from 80 kg・cm to 640 kg・cm, but have turned out weakest for fatigue strength.
- 社団法人日本材料学会の論文
- 1970-01-25
著者
関連論文
- ローラチェーンの疲れ強さに及ぼすブシュはめあい力とリンク数の影響
- ローラチェーンにおける疲労強度の統計的評価
- ローラチェーンの繰返し衝撃強度に及ぼすリンク数の影響
- 6・2・7ベルト・チェーン : 6・2機械要素 : 6.設計・機素・トライボロジー
- 偏心外力を受けるねじ締結体のコンプライアンスおよび内力係数について
- ねじ締結体の偏心締付け及び偏心外力下における疲労強度
- ローラチェーンの疲労強度とリンク数の関係
- ねじの疲労強度に及ぼす締付力および被締結体の影響
- ねじの塑性域締付けと疲れ強さ-4-
- ねじの塑性域締付けと疲れ強さ-3-
- ねじの塑性域締付けと疲れ強さ-2-
- ねじの塑性域締付けと疲れ強さ-1-
- ロ-ラチェ-ンの疲れ強さと元応力-4-
- ロ-ラチェ-ンの疲れ強さと元応力-3-
- ロ-ラチェ-ンの疲れ強さと元応力-2-
- ロ-ラチェ-ンの疲れ強さと元応力-1-
- 転造ねじの疲れ強さに及ぼす締付力及び予締付力の影響
- ねじ締結体の疲れ強さに及ぼす締付力および予締付力の影響
- ローラチェーンの疲れ強さに及ぼす元応力の影響
- ローラチェーンリンクプレートの予荷重及びブシュ嵌合力が疲労強度に及ぼす影響
- ねじの締付力と疲労強度
- ローラチェーンの予張力加工が疲労特性に及ぼす影響
- ローラチェーンリンクプレートの疲労および衝撃強度に及ぼす熱処理の影響
- チェーンリングプレートの疲れおよび衝撃強さに及ぼすショットピーニングの効果
- ローラチェーンリンクプレートの疲労強度に関する研究(リンクプレートの形状,ショットピーニングと孔部仕上について)