- 論文の詳細を見る
Low carbon-medium nitrogen 316 stainless steel(316FR)with improved creep strength was developed for structural material for the demonstration fast breeder reactor(FBR).Fatigue, creep-fatigue and creep crack propagation tests have been conducted using CT specimens of 316FR welded joints at 650°C in order to investigate the applicability of crack propagation evaluation methods to welded joints.The results obtained are as follows.The fatigue J-integral range of welded joints could be estimated using material data of the base metal by the simplified J-integral estimation methods, the reference stress method and the GE/EPRI method, when the crack opening ratio were considered.Heating time(testing time)made a difference in creep-fatigue and creep crack propagation rates estimated by the creep J-integral range.It was considered that the degradation of microstructure(from delta ferrite into sigmaphase)by high temperature aging, which reduced ductility, affected the crack propagation behavior.
- 社団法人日本材料学会の論文
- 2000-03-15
著者
関連論文
- 統計・確率論的手法に基づく複合領域における信頼性解析法の提案
- 212 改良SUS316鋼溶加材の開発研究
- 818 原子炉圧力容器・再循環配管系の圧力脈動挙動に関する研究
- はんだバンプ接合部の損傷パスシミュレーション : 機械的疲労試験条件での適用性検討
- はんだ接合部の損傷パスシミュレーション
- はんだバンプ接合部のき裂進展挙動評価(実験計測技術の新展開)
- SUS304切欠き試験片の高温における裂発生寿命
- はんだバンプ接合部の機械的疲労試験と寿命予測
- J積分簡易評価法に基づく表面き裂のクリープ疲労き裂進展評価
- 低炭素窒素添加改良316ステンレス鋼のクリープ特性
- クリープ疲労き裂進展に及ぼす中間保持の影響 : 除荷過程で中間引張保持のある場合
- 高速炉構造用SUS316鋼溶接継手のクリープ疲労き裂進展評価
- 表面き裂付配管のクリープ疲労き裂進展評価
- 236 複数表面欠陥からのクリープ疲労き裂進展評価
- 過応力概念を用いた改良 9Cr-1Mo 鋼のクリープ疲労寿命評価
- 改良9Cr-1Mo鋼の非弾性変形挙動への統一型構成式の適用
- 224 改良9Cr-1Mo鋼のクリープ疲労寿命評価(高温強度)
- 時間依存分離形構成式の陰的積分とコンシステント接線係数
- 725 非線形移動硬化を有する分離型構成式のSn-3.0Ag-0.5Cuへの適用(弾(粘)塑性構成式,塑性挙動のモデリングとシミュレーション-ナノからマクロまで-,オーガナイスドセッション5,第53期学術講演会)
- 714 多結晶モデルの有限要素解析における境界条件の影響(結晶塑性,塑性挙動のモデリングとシミュレーション-ナノからマクロまで-,オーガナイスドセッション5,第53期学術講演会)
- 309 Sn-3.5Ag はんだの疲労寿命に及ぼすひずみ波形の影響
- Sn-37Pbはんだのクリープ疲労き裂進展評価
- 414 Sn-Ag 系鉛フリーはんだのクリープ特性