常圧焼結窒化ケイ素の多軸応力下の破壊挙動(第2報)
スポンサーリンク
概要
- 論文の詳細を見る
Four-point shear bending tests were carried out at room temperature to study the fracture criteria for the large crack of sintered silicon nitride under a mixed-mode. The data of stress intensity factor under mode I and II agreed with the G-criterion. Ring-on-ring tests and ball-on-ring tests were also performed to investigate the fracture behavior of sintered silicon nitride under tension-tension equibiaxial stresses. The experimental results were compared with the predicted strength based on the Weibull statistical theory and various fracture criteria. The strength under tension-tension stresses agreed with the predicted strength based on shear sensitive criteria for natural flaw. In the previous work, the strength of sintered silicon nitride under tension-compression biaxial stresses agreed with the predicted strength based on shear insensitive criteria. In this paper, it was proposed that the modified G-criterion is applicable to the prediction methodology for fracture strength of ceramic component under both tension-tension and tension-compression biaxial stresses.
- 社団法人日本セラミックス協会の論文
- 1991-07-01
著者
関連論文
- A114 ディーゼルパーティキュレートフィルター内流動と微粒子捕集のミクロ観察と予測法に関する研究
- 半導体製造装置用セラミックヒータ
- チャネル構造を有する多孔質体における流動特性と表面セラミックス膜の影響(熱工学,内燃機関,動力など)
- 不透明物体内高圧ガス流動の非破壊・非侵襲MRI計測
- セラミックスの疲労(第3報) : 常圧焼結窒化ケイ素の高温繰り返し疲労挙動
- セラミックスの疲労(第2報) : 常圧焼結窒化ケイ素の室温における繰り返し疲労特性
- 常圧焼結窒化ケイ素の多軸応力下の破壊挙動
- セラミックスの疲労(第1報) : 引張-圧縮繰り返し応力下における常圧焼結窒化ケイ素の疲労挙動
- K-1220 磁気共鳴イメージングによる急縮流チャネル内粘土流動の計測(S17-5 複雑流体の流れ)(S17 非ニュートン流体の複雑流路内の流れ)
- 4626 超高温空間用流れセンサの開発(G06-5 熱・流動現象(1),G06 熱工学)
- 1040 セラミックス/金属接合体に生じる残留応力の定量的評価(その 2)
- 817 Al/Al_2O_3 拡散接合体に生じた残留応力の定量的評価とその特徴
- 多重モードワイブル分布を用いた窒化ケイ素の強度解析
- 常圧焼結窒化ケイ素の多軸応力下の破壊挙動(第2報)
- セラミックスの疲労(第4報) : 常圧焼結窒化ケイ素の引張応力下の静的疲労強度
- 多軸応力下のセラミックスの破壊強度 (エンジン用セラミックスの現状と将来展望--素材を材料として使いこなすために-1-)