安定化ZrO_2焼結体の微粒化とその機械的特性への影響
スポンサーリンク
概要
- 論文の詳細を見る
In order to investigate the effect of grain size on the mechanical properties of stabilized ZrO_2 ceramics, fine grained ceramics were prepared by adding carbon derived from novolak phenol resin by thermal decomposition. A stabilized ZrO_2 ceramic with an average grain size of 0. 6 μm and relative density of above 99% was obtained by adding 0.23 wt% of carbon and sintering at 1500℃. It was speculated that the carbon at grain boundaries prevents the grain growth of ZrO_2. Hardness and Young's modulus of the fine grained ZrO_2 ceramics were nearly the same as those with large grains. However, the fracture toughness of the fine grained ZrO_2 was smaller than that of large grained one, which may have resulted from the reduced crack deflection effect of increasing fracture toughness in fine grained ZrO_2 ceramics.
- 社団法人日本セラミックス協会の論文
- 1988-10-01
著者
-
前田 邦裕
(株)日立製作所日立研究所
-
三吉 忠彦
(株)日立製作所日立研究所
-
竹田 幸男
(株)日立製作所日立研究所
-
樋口 晋介
(株)日立製作所日立研究所
-
竹田 幸男
(株)日立製作所日立研究所:(現)ジャテック(株)
-
竹田 幸男
(株)日立製作所
関連論文
- V_2O_5-P_2O_5系ガラスの耐水性に及ぼすSb_2O_3添加の効果
- 家電製品の腐食実態と新腐食試験法ACTEの開発
- β-SiCの焼結過程における多計変化
- 高熱膨張性を示すZrO_2-CaF_2系複合セラミックスの熱的,機械的性質
- SiC焼結体の熱伝導率及び電気抵抗率に及ぼす焼結助剤の影響
- BeO添加SiC焼結体の特性に及ぼす製造条件の影響
- SiC焼結体の熱伝導率及び電気抵抗率に及ぼす焼結助剤の影響
- SiC焼結体中不純物の焼結温度依存性
- Bサイト比率を変化させたPb(Mg, Nb)O_3 系強誘電性セラミックス
- Y_2O_5-P_2O_5系ガラスの耐水性に及ぼす組成と添加物の影響
- 高熱伝導 SiC セラミックスの耐熱衝撃性
- 高熱伝導SiCセラミックスの機械的性質
- BoO添加SiC焼結体における電気絶縁性のキャリア濃度依存性
- SiCセラミックスにおける微小電極を用いた結晶粒内,粒界V-I特性の測定
- 安定化ZrO_2焼結体の微粒化とその機械的特性への影響
- 無加圧焼結SiC焼結体の熱伝導率及び電気抵抗率に及ぼす焼結助剤の影響
- Y-Ba-Cu-O系超伝導体の特性及び微構造観察(セラミック・レター)
- BeO及びAlN添加SiC焼結体の分析電子顕微鏡による焼結過程の検討
- SiC繊維強化Si_3N_4複合焼結体破壊挙動のその場観察