特殊鋼の疲勞並に衝撃破壊に於ける破壊起點の形状の影響に就て
スポンサーリンク
概要
- 論文の詳細を見る
Local breaking or sectional rupture of a steel construction during actual use, is caused by, in most cases, the fatigue introduced by some complicated and repeatedly applied force, moreover, it is well known fact that in case there are some notches, sharp curves or turnings in a steel body, the fatigue is accelerated. Considering that those complicated forces are the resultant of various simple forces, the writer made a simple repeated fatigue test using specimens having various shapes of notch or sharply curved sections, and the results are compared. According to those results, in case of tough construction special steels, it has been revealed that the influence notch angle, radious of the sharp corner of the specimen is quite remarkable, and this tendency is also shown by a simple impact test. Hence, the material and the shape of the construction in actual use have an intimate relation, therefore, selection of material and its heat treatment should be carefully considered. In general specification for steels, there has been set Charpy or Izo dimpact value, but the shape and demensions of the test piece are fixed ; so that the ordinary impact test value is not dependable specification for the selection of a material. A specified test piece having an inferior impact value exhibits a superior impact value, if the shape and position of application being properly designed, hence, in actual application of a given material, the above mentioned facts should be bone in mind.
- 社団法人日本鉄鋼協会の論文
- 1934-10-25
著者
関連論文
- 第2回ガスタービンに関する座談會記録 : 内燃機関部門主催
- ニッケルクロム鋼代用鋼座談會
- I.鉄鋼(機械用金属材料発達の展望)
- リムを超耐熱鋼 LCN-155 で作れる大型複合車盤の製造研究
- 136 リムを超耐熱鋼 LCN-155 で作れる大型複合車盤の製造研究(第 52 回講演大会講演大要)
- 構造用鋼に添加せらるる特殊元素の効果に就て
- 特殊鋼の疲勞並に衝撃破壊に於ける破壊起點の形状の影響に就て
- 3) 特殊鋼材の疲勞破壞並に衝撃破壞に於ける「切込み」の影響に就て(日本鐵鋼協會第拾貳囘講演大會)
- 鋼の纎維状組織と其の性質
- 鋼の変態時における異状変形
- 耐熱鋼-5-
- 耐熱鋼-4-
- 耐熱鋼-3-
- 耐熱鋼-2-
- 耐熱鋼-1-
- 耐熱鋼-8-
- 耐熱鋼-7-
- 耐熱鋼-6-