元素の電弧熔接に於ける特性
スポンサーリンク
概要
- 論文の詳細を見る
The author described in the "Tetsu to Hagane" Vol.XIV, No.7, p.577-595 that the are welding of cast iron is practicable only when barium carbonate is used so as to retard the fusion of electrodes. He now tested the effect of 48 elements besides barium, with the object of knowing the cause of retarding action. He coated mixtures of equal quantities of graphite and carborundum and of compounds of various elements on wrought iron bars, and connecting these bars first to the positive and then to the negative pole of the generator, he deposited cast iron. He measured the time, voltage, current and energy required to melt each electrode. He found that when the coated electrodes containing alkali metals or alkaline earth metals are connected to the negative pole of the generator, the fusion of the electrodes is regularly retarded in a successively increasing manner (i.e., greater energy is required), according as the atomic weight of either group increases. This action is especially marked with barium. The oxygen group produces an opposite effect, while halogen produces both effects. The other elements have no particular influence. The author next tested the relationship between the quantities of barium compounds and their respective retarding effect and found that the very small quantities of them are sufficient. The photograph of deposit metals obtained by connecting the electrodes to both poles of the generator, is shown.
- 社団法人日本鉄鋼協会の論文
- 1929-05-25
社団法人日本鉄鋼協会 | 論文
- 低圧タービンロータ用 3.5%NiCrMoV 鋼の長時間恒温焼戻脆化におよぼす不純物元素および Si, Mn 量の影響
- 超超臨界圧タービン用 12%Cr 鋼ロータのクリープ破断特性(新しい耐熱鋼)
- 628 18Mn18Cr 系オーステナイト鋼の機械的性質におよぼす N 量および冷間加工温度の影響 : 高 Mn Cr 系オーステナイト鋼の冷間加工に関する研究 2(二相ステンレス鋼, 非磁性鋼, 材料, 日本鉄鋼協会第 113 回(春季)講演大会)
- 627 18Mn5Cr 鋼の冷間拡管加工後の残留応力分布におよぼす拡管加工温度の影響 : 高 Mn Cr 系オーステナイト鋼の冷間加工に関する研究 1(二相ステンレス鋼, 非磁性鋼, 材料, 日本鉄鋼協会第 113 回(春季)講演大会)
- 582 鉄基耐熱合金大形ロータの性能(耐熱鋼・耐熱合金 (II), 材料, 日本鉄鋼協会第 111 回(春季)講演大会)