In the manufacture of DI can made of tinplate, macro non-metallic inclusions (NMIs) which exist on the flanging area of DI can cause cracks in flanging. It is difficult to observe NMIs on the surface of tinplate because they usually exist in the inner part of the steel sheet. The magnetic-particle testing can detect NMIs, but it is difficult to determined the size of NMIs quantitatively. This paper describes the quantitative determination of the size of NMIs by using the magnetic leakage flux testing, and the influence of NMIs on the flanging cracks. Flanging crack ratio in continuous DI can-making test are in proportion to numbers of NMIs obtained in this test is in good agreement with the theoretical results. Conclusively, the number of NMIs per unit area detected on the part of the coil by the magnetic leakage flux testing enable us to estimate the flanging crack ratio of the coil before DI canmaking.
- 社団法人日本鉄鋼協会の論文
- 1982-01-01
著者
-
藤井 昭明
東洋鋼鈑(株)下松工場
-
中島 厚
東洋鋼鈑(株)下松工場
-
藤井 昭明
東洋鋼鈑株式会社下松工場
-
御園生 一長
東洋鋼鈑(株)技術研究所
-
福元 亮一
東洋鋼鈑(株)技術研究所
-
藤井 昭明
東洋鋼鈑(株)技術研究所
-
福元 亮一
東洋鋼はん 技研
関連論文
- 177 蛍光 X 線によるすずめっき量の連続測定(分析, 加工・性質・分析, 日本鉄鋼協会 第 81 回(春季)講演大会)
- 150 連続磁気硬度計(性質, 日本鉄鋼協会第 69 回春季講演大会講演論文集 (II))
- 62 帶鋼冷間圧延の作業條件の研究 (III) : ロール及び帯鋼の温度について(第 49 回講演大会講演大要)
- DI 缶のフランジ割れにおよぼす大型介在物の影響
- 274 光沢複合電気亜鉛めつき鋼板の光沢測定(表面処理・腐食, 性質, 日本鉄鋼協会 第 95 回(春季)講演大会)
- 175 表面電位計の鉄鋼板表面研究への応用(分析その他, 日本鉄鋼協会第 64 回(秋季)講演大会講演大要)
- (5) β線厚み計及び鍍錫量測定装置について(日本鉄鋼協会中国四国支部第 1 回鉄鋼技術発表会演題の概要)
- 32 β線走間帯鋼厚み計に就て(日本鐵鋼協會第 48 回講演大會講演大要)
- 32 β線によるブリキ板の鍍錫量測定裝置に就て(日本鐵鋼協會第 47 囘講演大會講演大要)
- 508 薄めっきぶりきの DI 加工性(計測・検査・缶用鋼板, 加工システム, 日本鉄鋼協会第 106 回(秋季)講演大会講演)
- 超硬合金のSinter-HIP処理
- 479 イージーオープンエンド用鋼板の開発(電気亜鉛系めつき, 缶用材料, 加工・システム, 日本鉄鋼協会第 108 回(秋季)講演大会)