低合金鋼の遅れ破壊におよぼす焼もどし, 前オーステナイト粒度, 試験片形状の影響
スポンサーリンク
概要
- 論文の詳細を見る
Effects of tempering condition, prior-austenite grain-size, and shape of test specimen on the behavior of hydrogen-induced delayed fracture have been investigated for several low alloy steels for high strength bolt. The main results are as follows ; (1) The tempering at temperatures above 500℃ improves the resistance to delayed fracture, except for secondary hardenable steels. This resistance depends on the strength level and the strain hardening behavior. (2) Both steels with fine (ASTM 9-10) and coarse (ASTM 0-3) grains of prior-austenite have a tendency to be more susceptible to delayed fracture than these with medium grain size (ASTM 4-5). (3) The thinning of specimen width results in decreasing of the susceptibility to delayed fracture owing to the change of stress condition, from plain strain to plain stress.
- 社団法人日本鉄鋼協会の論文
- 1972-03-01
著者
関連論文
- レール頭頂面変形層における集合組織の発達について(X線材料強度小特集)
- 771 レール転動面の塑性変形状態(工具・金型・マルエージ鋼・レール・軸受鋼, 材料, 日本鉄鋼協会第 110 回(秋季)講演大会)
- 643 レールの転動接触面下の変形挙動(ロール・レール, 鋼管, 材料, 日本鉄鋼協会第 108 回(秋季)講演大会)
- 567 レールの転動接触面の塑性変形状態(マルエージ・工具鋼・ロールレール, 材料, 日本鉄鋼協会第 106 回(秋季)講演大会講演)
- 604 レール鋼の高速転動疲労試験(照射脆化・液体脆化・レール・潤滑, 材料, 日本鉄鋼協会第 104 回(秋季)講演大会)
- 415 低合金レール鋼の疲労き裂進展特性(疲れ・マルエージ鋼・他, 性質, 日本鉄鋼協会 第 97 回(春季)講演大会)
- 695 高力ボルトの遅れ破壊曝露試験(硫化物・腐食割れ・おくれ破壊・腐食, 性質, 日本鉄鋼協会 第 100 回(秋季)講演大会)
- 討 37 焼もどしマルテンサイト鋼の水素による粒界破壊機構(V 鉄鋼の水素脆化機構, 第 105 回講演大会討論会講演概要)
- レール鋼の繰返し打撃による塑性変形挙動
- 橋梁における高力ボルトの遅れ破壊
- 高強度鋼の遅れ破壊におよぼすミクロ偏析の影響
- 754 橋梁における高力ボルトの遅れ破壊 : 事例研究(水素脆性, 材料, 日本鉄鋼協会第 104 回(秋季)講演大会)
- 635 高強度鋼の遅れ破壊に及ぼす粒界偏析の効果(疲れ・遅れ破壊・非磁性鋼・レール, 性質, 日本鉄鋼協会第 102 回(秋季)講演大会)
- 485 高強度鋼の遅れ破壊試験法のための一検討(第 1 報) : 試験片形状および試験片採取法の効果(ラインパイプ・応力腐食割れ, 性質, 日本鉄鋼協会 第 99 回(春季)講演大会)
- 低合金鋼の遅れ破壊におよぼす焼もどし, 前オーステナイト粒度, 試験片形状の影響
- 225 焼もどしマルテンサイト鋼の遅れ破壊におよぼす前オーステナイト粒度の影響(脆性・靱性・低温用鋼, 加工・性質・分析・計測, 日本鉄鋼協会第 80 回(秋季)講演大会講演)
- 257 低合金鋼の遅れ破壊におよぼす前オーステナイト粒度の影響(腐食・表面処理・高張力鋼, 性質, 日本鉄鋼協会 第 78 回(秋季)講演大会)