高速度鋼の水鈍
スポンサーリンク
概要
- 論文の詳細を見る
Furnace-cooling is a standard practice for annealing high-speed steels. It constitutes, however, a bottle-neck to production because of a long time required for the operation. To expedite and simplify the operation, the authors conducted many experiments. Earlier, stepped annealing or isothermal annealing had been found effective. This time, effectiveness of water annealing was confirmed. The experimental results testify that : 1. Water annealing with the heating temperature 800℃ held for 120mn. will effectively soften quenched high-speed steels with more rapidity and simplicity. The softened degree falls certainly short of complete annealing but comes up well to the hardness obtainable through machining. 2. Five to six times of water annealing operations will ensure softening if the following cycle is repeated : water cooling after rapid heating is applied and the heat is held for a brief time. Oil annealing should be recommended for the works of large dimensions or complicated contours.
- 社団法人日本鉄鋼協会の論文
- 1955-11-01
著者
関連論文
- 疲れ破壊の実例(疲れおよびクリープ特集)
- 電解焼入法について
- スパークテストにおける羽毛状火花
- 疲れ破面の金属組織学的考察
- 高速度鋼の水鈍
- 84 高速度鋼の水鈍(第 49 回講演大会講演大要)
- プレステンパーについて
- 93 タイヤのブレーキバーンに就て (III)(日本鐵鋼協會第 45 回講演大會講演大要)
- 86 ブレステンパーについて(日本鐵鋼協會第 45 回講演大會講演大要)
- タイヤのブレーキ・バーンに就て
- 燒入硬度に及ぼす肉厚及びコーナ部の影響
- 鋼材の火花試験法 : (第9回講習會(機械材料その他)記録(その4))
- 工具鋼の熔接(熔接講習會記録(その6))
- 398 低炭素鋳鋼品の炎焼入れによる耐摩耗性の効果(変態・析出・熱処理, 性質, 日本鉄鋼協会 第 86 回(秋季)講演大会)
- 301 鋳鋼品の摩耗試驗と熱処理効果(鋼管・オースフォーミング鋼・疲労・摩耗, 加工・性質・分析, 日本鉄鋼協会 第 82 回(秋季)講演大会)
- 高速度鋼の連続冷却変態曲線について-1-
- 亜急熱焼入鋼の機械的性質について-1-
- オーステンパーおよび焼入焼戻による鋼の機械的性質の相違について-3-
- 鉄道用鋼材の趨勢