YAGレーザによる銅合金の接合特性
スポンサーリンク
概要
- 論文の詳細を見る
This paper describes how the lapped spot welding of copper alloy material for structural components is performed with a YAG laser. Welding conditions and their relation. to mechani-cal characteristics and metal structures is examined. The main results of this paper are summarized as follows : (1) Laser power, amount of defocus and welding strength are deter-mined by using newly introduced equations. (2) Laser powex' is 10-12.5 J, amount of defocus is ±1mm, and the pulse duration is 1-3 ms. With these conditions, a welding strength of over 150 N is obtained. (3) The welded part of the metal structures is dendrite. This clarifies the validity of the metal structures and hardness characteristics under YAG laser operating conditions.
- 公益社団法人精密工学会の論文
- 1985-08-05
著者
関連論文
- 202 タングステンワイヤロープの機械的強度
- 201 ステンレス鋼ワイヤロープの熱処理矯正
- アレーベア光ファイバーの一括端面加工
- 光ファイバの端面研磨と加工変質層 : 加工変質層と反射減衰量の関係
- プリンタ用紙の加工特性 : 孔がれ・打抜き・引張切断
- 用紙におけるスプリングバックと折りたたみ特性
- プリンタの最適折りたたみと用紙特性
- 小形印字ヘッドにおけるYAGレーザ溶接加工
- 135 YAGレーザによる精密溶接 : 予熱効果について(溶接)
- 309 用紙の加工特性の実験的検討(高分子材料)
- 202 YAG レーザによる重ね合せ溶接に関する一検討
- 134 超硬およびタングステン細線の引張り, 疲れ, ねじり破面について
- 207 ステンレス鋼ワイヤロープの機械的強度に及ぼすプーリ曲げの影響
- 131 ウレタン系歯付ベルトの寿命試験
- 2-20 ステンレスワイヤロープの機械的性質
- YAGレーザによる銅合金の接合特性